PE Shrink Film for Corrugated Carton Packaging: A Specification Solution

Nov 10, 2026 Leave a message

Solution at a glance

Film: virgin-resin PE heat-shrink film, thickness in four weight tiers from 30–50 μm up to ≥100 μm; shrinkage range 30 %–70 %, transverse 5 %–15 %, machine direction 60 %–70 %.

Web width is the hard constraint: maximum production web width 1800 mm; single-layer flat film wraps a maximum perimeter of about 1565 mm. Larger cartons move to a hood or tube-film solution; single-carton wrapping is not attempted.

Process: sealing bar 120–180 ℃, shrink tunnel 140–200 ℃, matched to the weight tier. For cartons, run the higher temperature and the shorter dwell, trial first, then batch.

Delivery: samples in 1–3 days, standard lead time 7–15 days, with on-site training, custom formulation, and free on-site servicing.

1. Scope and the problems addressed

The solution applies to cartons that are already formed and ship as a whole case or a whole pallet load. It does not apply to bulk, unpackaged, or vacuum-fresh products. A carton is rigid, has edges and corners, and absorbs moisture, so its shrink process is not identical to that of soft packaging. Three things are judged together: carton dimensions, weight per unit, and surface condition.

1.1 Four typical carton packaging scenarios

Scenario Typical goods Pack format Key risk
Single-carton wrap Bottled water, beverages, beer, household chemicals by the case Single-layer flat film sleeved on, shrunk in a sleeve wrapper Corners punching through the film, seal opening
Multi-carton bundle 2×2 and 2×3 case groupings, gift boxes, e-commerce shipments Whole bundle wrapped after grouping, L-sealer plus shrink Bundle seams shifting, unit coming loose
Pallet hood Pallet freight, building boards, machinery parts Tube film or five-sided hood over the whole load Pallet corners puncturing, stack instability
Irregular and heavy goods Furniture, hardware, large machinery Heavier film with corner boards, high tunnel temperature Insufficient film, incomplete shrink

1.2 Six carton-packaging problems and the matching capability

Problem Solution response What acceptance looks at
Cases coming apart, tape residue Full-perimeter shrink wrap replaces tape; case and lid become one Cannot be pulled apart, no tape residue on the surface
Moisture and dust in transit Six-sided coverage, moisture and dust barrier No breaches, no water marks on the carton
Corners and flute cuts puncturing the film Puncture-resistant formulation, upper end of the thickness tier, corner boards where needed Number and location of damage points in the first-article full inspection
Colour cartons and white cartons need a uniform look High-clarity, low-haze film, optional seven-colour rotogravure printing Haze and print register, compared against the signed sample
Too many consumable items, slow manual packing One roll replaces tape plus stretch film; two operations become one Packing time per carton, number of consumable SKUs
Export and recyclability requirements Virgin resin, food grade, and recyclable regrind options; food grade supplied with an SGS report Material declaration and test report

2. Film selection and process window

2.1 Thickness in four tiers by weight per unit

Thickness and temperature are a matched pair: set the tier by weight per unit first, then take the temperature for that tier. Do not adjust one without the other. The production range of the company's PE shrink film is 30–300 μm, with thickness tolerance held to ±10 μm.

Weight per unit Recommended thickness Sealing bar Shrink tunnel Carton fit
Under 1 kg 30–50 μm 120–160 ℃ 140–160 ℃ Light small cartons, gift boxes, small daily items
1–5 kg 60–75 μm 140–160 ℃ 160–180 ℃ The main tier for beverage and household-chemical single-carton wrapping
5–10 kg 80–100 μm 160–180 ℃ 180–200 ℃ Multi-carton bundles, hardware and parts cartons
Over 10 kg ≥100 μm Set at the machine limit 180–200 ℃ Pallet loads, furniture and large machinery

Three additional corrections apply to cartons: where corners are hard or the pack carries a wooden pallet or hardware, take the upper end of the tier; for colour cartons, laminated or varnished surfaces, trial 2–3 units before a batch; where carton moisture content is high, air and dehumidify before wrapping. These three change which value inside the tier is used - not the tier itself.

2.2 Web width decides whether flat film can wrap a single carton

Estimate the film width as follows: maximum perimeter = 2 × (carton length + carton width); required film width = two thirds of the height + length. The company's maximum production web width is 2500 mm.

2.3 Three process constraints specific to cartons

Higher temperature, shorter dwell. A carton held too long in the heat takes up moisture, softens, and its glue lines open. Leave the tunnel as soon as shrinkage is complete; do not compensate for incomplete shrink by extending the heat.

Adjust speed and temperature together. Running too fast leaves the wrap loose; running too slow splits the side wall. The two are cause and effect on each other - change one variable at a time and record it.

Add perforations where needed. Air trapped inside the film pushes against the carton face and forms a bulge; a higher perforation density improves venting, but too dense a pattern weakens the moisture barrier. Set it from the trial run.

2.4 Printing and brand presentation

Where the brand must appear, the film can be printed single-colour to multi-colour rotogravure. The company runs three seven-colour rotogravure presses with a daily printing capacity of 800,000 metres. The printable width of printed film is likewise limited to a 1200 mm web; once artwork is final, pricing is checked against it and lead time confirmed. A colour carton that already carries printed artwork usually takes clear film so the carton information stays legible, with no second layer of print.

3. The selection path

The order is fixed in three steps: measure the carton to set film width, weigh the unit to set thickness, then correct by carton risk and machine temperature control. Width comes first because it is a hard capacity constraint - beyond it, only the film format can change. Thickness still has room to move inside a tier, so reversing the order is what produces the rework case of "thickness chosen, width impossible".

Step Judge → set Basis What to change at the limit
① Measure carton → set film width Required width = two thirds of height + length Perimeter beyond what single-layer flat film can wrap: move to hood or tube film
② Weigh unit → set thickness Under 1 kg: 30–50 μm, tunnel 140–160 ℃; 1–5 kg: 60–75 μm, tunnel 160–180 ℃; 5–10 kg: 80–100 μm, tunnel 180–200 ℃; over 10 kg: ≥100 μm, tunnel 180–200 ℃. Thickness tolerance ±10 μm. Required thickness above 300 μm, or no room left in the tier: change film format or add corner boards - do not keep thickening to compensate
③ Read the carton → correct parameters Hard corners, wooden pallet or hardware: upper end of the tier, corner boards where needed; colour, laminated or varnished carton: trial 2–3 units before a batch; high moisture: air and dehumidify first; the existing tunnel must cover 140–200 ℃ Any one unmet: resolve before batch running, do not force it inside the same tier

The three steps converge on one specification sheet: film specification (format - flat, tube or hood - width, thickness, whether printed), process parameters (sealing bar temperature, tunnel temperature, conveyor speed, whether perforations are needed for venting), and the trial baseline (damage locations from the first-article full inspection, actual shrink result, film length consumed per carton).

4. Configuration by scenario

Scenario Film specification Equipment Parameter focus Risk control
Single-carton wrap Single-layer flat film, 60–75 μm Sleeve wrapper with shrink tunnel Sealing bar 140–160 ℃, tunnel 160–180 ℃ Film width at perimeter × 1.15; upper thickness at the corners
Multi-carton bundle Single-layer flat film, 80–100 μm L-sealer plus shrink Sealing bar 160–180 ℃, tunnel 180–200 ℃ Position the bundle before shrinking so it cannot shift
Pallet hood Tube film or five-sided hood, ≥100 μm Hood machine or heat gun Tunnel 180–200 ℃, even heat from the top down Corner boards on all four pallet corners; hood only after the stack is stable
Irregular and heavy goods ≥100 μm, puncture-resistant formulation Sleeve wrapper or heat gun Tunnel 180–200 ℃ Sand wooden-pallet burrs; protect protruding parts with corner board first

Where one customer has several carton sizes, write a specification per carton size rather than merging them into one "general specification". Two cartons with close widths can share a roll, but thickness must follow each one's weight tier, so a heavy carton never ends up on thin film.

5. Film consumption and cost per carton

Estimation model: film mass per carton (kg) = film width (m) × film length used per unit (m) × thickness (m) × 0.925, where 0.925 is the density of PE (kg/m³), and the film length per unit is taken as "carton height + carton width × 2 × 1.1", the 1.1 covering seal and fold allowance. Unit price follows virgin-resin grade and varies with thickness, order quantity and destination.

6. Quality control and acceptance

Acceptance has two layers: incoming film is checked against the company's standing criteria, and wrap performance is baselined on the customer's own production trial. The first layer is the standard; the second is that customer's real condition. Both are recorded.

Item Criterion Method Decision
Thickness 30–300 μm, tolerance ±5 μm Micrometer at 5 points across the web Deviation within ±5 μm on the same roll
Width and lay-flat Per order specification Tape measure at three positions Matches the order
Shrinkage Range 30 %–70 %, MD 5 %–15 %, TD 60 %–70 % Marked line, then through the tunnel or hot water Within range, all four corners covered
Seal strength As agreed between the parties Peel the seal, short-drop the whole carton No false seal, no perforation
Appearance High clarity, low haze, flat wind Visual, compared against the signed sample No perforation, no clustered gels, no colour deviation
Wrap integrity Six faces covered, no breach Full inspection on the first batch, sampling after stabilisation Zero breaches

7. Route to production

Of the five steps, the first three decide whether the solution holds, the fourth decides whether it can run as a batch, and the fifth decides whether the line can handle exceptions itself. Sampling is mandatory; batch parameters are not set from sample photographs alone.

Figure 2: the five-step route to production for carton PE shrink film packaging, with responsible party, deliverables and pass condition for each step.

8. Common faults and handling

Symptom Main cause Handling Prevention
Loose, incomplete shrink Tunnel temperature low; conveyor too fast Raise 5–10 ℃; slow down and increase perforation density Set temperature by weight tier, trial before each shift
Side wall splitting Tunnel temperature high; conveyor too slow Lower 5–10 ℃; speed up Adjust temperature and speed together
Burned holes at the seal Sealing bar too hot; bar contaminated Lower temperature or raise speed; clean the bar Clean the bar every shift, trim temperature
Carton deforming, glue line opening Dwell too long, carton repeatedly heated Shorten dwell, raise temperature to shrink quickly Trial 2–3 colour cartons before a batch
Ink transfer, mottled film surface Ink not dry; temperature too high Wrap after the ink dries, lower temperature Separate printing and wrapping in time
Condensation inside the film Carton moisture high, large in-out temperature difference Air and dehumidify, cool slowly after wrapping Confirm the carton is dry before storage
Corner puncture Wooden-pallet burrs, hard carton edges Sand burrs, add corner board, thicken within the tier Record damage points in the first-article inspection

9. Delivery, service and commercial terms

Item Terms
Minimum order No rigid MOQ; small trial orders and long-term volume both supported
Sampling Sample made and shipped within 1–3 days
Lead time 7–15 days for standard orders; urgent orders can be scheduled ahead to shorten the cycle
Production limits Web width up to 1800 mm, thickness 30–300 μm, annual PE shrink film capacity 15,000 tonnes
Trade terms FOB Shanghai as standard; CIF, DDU and DDP supported
Certification ISO 9001 quality management system; SGS test report supplied for food-contact cases
Technical service Equipment operating manual, fault-handling video library, engineer on-site hands-on training, free on-site servicing (parts supplied by the customer), film formulation customised to product dimensions and machine parameters
Service radius Jiading, Shanghai plant as the base, covering Jiangsu and Zhejiang with same-day engineer travel
Storage Store at −15 ℃ to +40 ℃, dry, ventilated, away from light and heat sources; use summer stock within 2 months and winter stock within 6 months; turn each roll every 3 months to prevent single-side compression
Quotation Resin, printing, processing and freight listed separately; no hidden charges

10. Boundaries, risks and open items

10.1 Six boundaries of the solution

Moisture barrier has a ceiling. PE shrink film suits moisture and dust protection in transport and storage; it is not a high-barrier pack. For long-term high humidity and heavy condensation inside sea containers, add desiccant or an inner moisture-barrier bag.

Tamper evidence is "easy to spot", not prevention. Once shrunk, the seal is continuous and opening leaves a clear trace, but the film cannot stop a tear and does not replace a security seal or an anti-counterfeit label.

Food contact requires food grade. Standard industrial film must not contact food directly; food packaging takes food-grade film with an SGS report.

It does not replace stretch wrap. PE shrink film conforms by heat; stretch film holds a pallet by tension. Different resin, different equipment, different application - the two are not interchangeable.

Carton heat tolerance and moisture set the limit. Prolonged high heat makes the carton take up moisture, deform and open at the glue line; cartons with high moisture content must be treated first, otherwise condensation mottling appears inside the film.

10.2 Seven items the customer needs to provide

Carton type and dimensions (length, width, height), weight per unit, whether a pallet is included.

Daily and peak output, existing equipment model and tunnel temperature range.

Carton material and flute count, moisture condition, whether colour-printed, laminated or varnished.

Whether a logo and colour matching are needed, and whether artwork is final.

Target acceptance criteria (damage rate, appearance, seal) and current customer complaints.

Whether food contact applies, destination country and transport mode - these decide food-grade material and trade terms.

Target unit price and annual volume, and whether a hood or tube format is acceptable.

With all seven in hand, the solution can be reduced to concrete specifications and a quotation within one working day. Missing any one of them, only a recommended specification can be issued - a firm lead time and unit price cannot.

Shanghai Ruiyue Plastic Products Co., Ltd. · Jiading, Shanghai · PE / POF shrink film